General Information for Steel A34-2
Material Group |
P - Steel |
Sub-Group |
Low Carbon Steel |
Tensile Strength |
300-500 [N/mm^2] |
Machinability |
65% - 80% |
Equivalent International Designations for Steel A34-2
Standard |
Name |
WNR |
1.0028 |
DIN |
Ust34-2 |
ANFOR |
A34-2 |
UNI |
Fe330Fe/330BFU |
JS1 |
SS330 |
Chemical Composition for Steel A34-2
Sorry, Not Availble for this Material
Cutting Speeds Recomendations for Non-alloyed steel 0.1-0.25% Carbon
Application |
Vc (m/min) |
Vc (SFM) |
Turning |
285-350 |
930-1150 |
Milling |
175-220 |
570-720 |
Parting |
135-170 |
440-560 |
Grooving |
160-195 |
520-640 |
Drilling |
115-140 |
380-460 |
Important! The speed estimation is given for an ideal situation:
- Most suitable carbide grade
- Stable tool clamping
- Stable workpiece clamping
- Good quality raw material
- A short overhang of the cutting tool.
- Nominal hardness of the material.
- etc.
Recommended Carbide Grades for Steel A34-2
Grade for Milling (Indexable)
Recommended Insert Cutting Edge Geometry for Steel A34-2
Honing Siz |
0.05-0.08 mm / 0.002-0.003" |
Rake Angl |
11° -13° |
Land Angl |
Positive |
Land Widt |
0.20-0.30 mm / 0.008-0.012" |